popular choices; Nouryon Trigonox 263 Arkema Luperox CAT730 United Norox MCP75 They're all MEKP / CHP blends.
Reach out to us, we might make a deal for some of your eq.
Bench bottom; Gelcoat 450g CSM 450g CSM 12mm core 450g CSM 450g CSM Bench back; same, no core. You could possibly eliminate the core in the...
For the cost, I'd just run basalt.
The sample on the right is much poorer quality construction. Weave is very inconsistent. May not comply with ISO.
We are an industrial composites manufacturer specializing in B2B production work located near Charleston, South Carolina, United States of...
The designer was heavily influenced by original MAGNUM pump designs (VLS/MLS), so the design philosophy is based around long strokes at slow drive...
Sunlight and humidity is what kills fiberglass. The treatment applied to cause the resin to uptake in the fibers is water soluble. If it gets...
There’s some unique challenges working overseas. My big suggestion I can have for you; Make sure your bill of materials is accurate, so you can...
Not as good as it could be. They only implemented about 30% of my suggestions, the ones that didn’t cost anything. I had a lot of low cost...
That mold set was over $120k and killed two ownerships from lack of profitability due to excess labor requirements. I was hired to do consulting...
then you’re paying a significant premium for something you’re not using. also, it will upset the ergonomics of the molding, which will reduce...
you can only laminate half the mold at a time. if you rotate it before curing, all of the material will fall down. non-issue with traditional mold.
still a female mold, but think more like a bathtub. With a rotating mold, the cycle time is doubled because each half of the molding must cure...